Plywood

Transmitting the glow of Indian homes, our wide scope of exemplary strong wooden gates are made utilizing predominant quality made from 100% seasoned wood that guarantees toughness, strong strength, superior quality and the smooth surface that provides an aesthetic appeal and remarkable bonding of plywood . Modi Udyog is known for their high quality.

Veneers from high-quality logs are selected and peel off on automated peeling machines. High quality resins are used for gluing the veneers make Nacro plywood safe. Plywood are made of 100% gurjan faced. The strong wooden entryways are accessible at exceptionally reasonable costs.

Transmitting the glow of Indian homes, our wide scope of exemplary strong wooden gates are made utilizing predominant quality made from 100% seasoned wood that guarantees toughness, strong strength, superior quality and the smooth surface that provides an aesthetic appeal and remarkable bonding of plywood . Modi Udyog is known for their high quality.

Veneers from high-quality logs are selected and peel off on automated peeling machines. High quality resins are used for gluing the veneers make Nacro plywood safe. Plywood are made of 100% gurjan faced. The strong wooden entryways are accessible at exceptionally reasonable costs.


PLYWOOD SPECIFICATION

Dimensions
(CL.8.)
a.) Length:
+6mm
-0mm
b.) width:
+3mm
-0mm
b.) Thickness:
±10% less than 6 mm
± 5% above 6 mm
d.) Squareness 0.2%
e.) Edge Straightness 0.2%
Test
1.) Glue Adhesion (CL.11.2)
2.) Water Resistance
(CL –11.2.3)
BWR grade boiling in water 8 hrs & dried for 16 hrs at 65±20C & followed six more cycles
MR grade submerged in water at 60 ±20C for 3 hrs and dried for 8 hrs at temperature 65±20C & then followed same two cycles
After then as per IS:1734 part 5 Adhesion of plies
3.) Mycological
(CL 11.2.2)
Sawdust charged with spores of the commonly ,wood destroying fungi & maintained the temp. 27 ±20C for a period of three weeks Adhesion of ply.
4.) Moisture Contents
CL 11.3
5 to 15%
Static Bending Strength
CL 11.4
Along the grain Across the grain
Grade BWR
MOR N/mm 2 MOE N/mm 2 MOR N/mm 2 MOE N/mm 2
Ind Ave Ind Ave Ind Ave Ind Ave
30 40 5000 4500 20 18 2200 2500
Test Result
Grade MR Along the grain Across the grain
MOR N/mm 2 MOE N/mm 2 MOR N/mm 2 MOE N/mm 2
Ind Ave Ind Ave Ind Ave Ind Ave
27 30 3600 4000 13 15 1800 2000
32 49 4875 4652 22 35 2954 3652
Workmanship & Finish (CL.9) 1.) Plywood board shall be of uniform thickness within the tolerance limit
2.) Faces of plywood board shall be reasonably smooth and face veneers shall be of reasonably uniform thickness.

© 2025 Nacro Plywood. All rights reserved. Designed & Developed By AVAMEDIA DESIGN